S&E Specialty Polymers GA-1046-80E PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-1046-80E PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A high-grade 80° C semi-rigid PVC insulation compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 64 - 70
64 - 70
ASTM D2240
Tensile Strength 26.0 MPa
3770 psi
ASTM D412
Elongation at Break 275 %
275 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 29 %
29 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1000 Hz
3.8

@Frequency 1000 Hz
ASTM D150