Material Notes:
SABIC INP108 is a high rubber ABS impact modifier resin, and is based on polybutadiene rubber. Offers superior impact efficiency, especially at low temperatures. Reduces notch sensitivity when alloyed with engineering polymers. Disperses easily. Provides abrasion and chemical resistance to polymers.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Volatiles 0.10 %
0.10 %
Total NA Volatiles; SABIC Method
Particle Size 400 µm
400 µm
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Descriptive Properties Value Comments
Rubber 32%
SABIC Method