Quadrant EPP Acetron® LSG POM-C, LSG grade, extruded (ISO Data)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Acetron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Acetron® LSG POM-C, LSG grade, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Within its portfolio of Life Science Grade Engineering Plastic Products - specifically developed for applications in the medical, pharmaceutical and biotechnology industries - Quadrant offers ACETRON® LSG biocompatible engineering plastic POM-C stock shapes for machining with certified ISO 10993 compliance High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stability (low water absorption) Good sliding properties and wear resistance Excellent machinability Good electrical insulating and dielectric properties Physiologically inert (most grades are suitable for food contact) Not self-extinguishing
Mechanical Properties Metric English Comments
K Factor (ISO) 45 µm/km
45 µm/km
Coefficient of Friction, Dynamic 0.30 - 0.45
0.30 - 0.45
Compliance Properties Metric English Comments
3A-Dairy No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable