Material Notes:
Wear resistant acid leached fiberglass. Heavy cloth.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1630 °C
2970 °F