Material Notes:
Pyrocast PT-60 is a ceramic fiber based insulating castable with very low thermal conductivity and excellent resistance to thermal shock.ApplicationsLaunder linings Distributor pan linings Ladle linings AdvantagesIn situ casting Excellent insulation characteristics Does not require pre-heating Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.800 g/cc
0.0289 lb/in³
oven dried
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000600 GPa
0.0870 ksi
Compressive Strength 0.800 MPa
116 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.210 W/m-K

@Temperature 800 °C
1.46 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1320 °C
2410 °F
Shrinkage 0.200 %

@Temperature 815 °C,
Time 18000 sec
0.200 %

@Temperature 1500 °F,
Time 5.00 hour
Component Elements Properties Metric English Comments
Al2O3 37 %
37 %
CaO 14 %
14 %
Fe2O3 4.0 %
4.0 %
Other 3.0 %
3.0 %
SiO2 41 %
41 %
TiO2 1.0 %
1.0 %