Material Notes:
A-1 rope core with jacket and mounting flange of densely woven glass cloth or wire reinforced glass cloth.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.800 g/cc
0.0289 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 540 °C
1000 °F
Users viewing this material also viewed the following: