Material Notes:
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application. This compound has obtained conformance to Cytotoxicity tests under ISO 10993-5 GUIDELINES, when combined with Trans 1756 pigmentation.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 sec; ASTM D2240
Tensile Strength at Break 17.2 MPa
2490 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Descriptive Properties Value Comments
Agency Ratings CPSIA Compliant
FDA Food Contact, Unspecified Rating
ISO 10993 Part 5
Appearance Clear/Transparent
Features Food Contact Acceptable
Non-Phthalate Plasticizer
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Medical Appliances
Users viewing this material also viewed the following: