PolyOne Geon™ 180 Series 180X7 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 180 Series 180X7 Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Geon® 180X7 is low molecular weight homopolymer resin that provides good chemical foam characteristics with excellent overblow resistance. The modified rhelogy of Geon® 180X7 provides increased viscosity and yield. Geon® 180X7 is recommended for applications where high Brookfield Viscosity and yield are required such as higly plasticized low density chemically blown foams, highly plasticized formulations, and weather stripping.Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 180X7, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390 (formulation): 100phr Geon® 180X7, and 60phr DOPInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Bulk Density 0.400 g/cc
0.0145 lb/in³
Fineness 4.5
4.5
Hegman, North Fineness; Geon® 390
Relative Viscosity 2.2 cP
2.2 cP
Correlation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 10.6 cP
10.6 cP
Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
11.8 cP
11.8 cP
One Day Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
19.8 cP
19.8 cP
Initial Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
23.3 cP
23.3 cP
One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 0.90
0.90
Inherent; ASTM D1243-60-A
Melt Flow 132 g/10 min

@Pressure 0.655 MPa
132 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
Mechanical Properties Metric English Comments
Tensile Strength 18.4 MPa
2670 psi
Optimum; With provided formulation; ASTM D638
Optical Properties Metric English Comments
Gloss 91 %
91 %
60 Degree Fused 5 mins @ 350FGeon® ALTC 65 (with provided formulation); Internal Method
Transmission, Visible 85 %
85 %
Geon® ALTC 66 (with provided formulation); Internal Method
Processing Properties Metric English Comments
Moisture Content 0.060 %
0.060 %
Karl FisherGeon® STP 683; Internal Method
Descriptive Properties Value Comments
Features Foamable
High Viscosity
Low Molecular Weight
Plasticized
Forms Powder
Fine, White Powder
Gel Temperature 72 °C
Internal Method; Geon® ALTC 29 (with provided formulation)
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 65
Internal Method; Correlation, 0.5gm/100ml
Methanol Extractables 3.5%
Internal Method; Geon® STP 894
Polymerization Process Microsuspension
Processing Method Plastisol
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Residual Vinyl Chloride Monomer < 9 ppm
Internal Method; Geon® STP 1005
Uses Foam
Weatherstripping