Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compounds feature unique high melt strength and shear thinning characteristics compared to conventional TPE materials for enhanced processability in extrusion applicationsInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.878 g/cc
0.878 g/cc
ASTM D792
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 190 °C
11 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
10 sec; ASTM D2240
64
64
ASTM D2240
Tensile Stress 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
510 mm/min; ASTM D412A
3.52 MPa

@Strain 200 %
511 psi

@Strain 200 %
510 mm/min; ASTM D412A
4.03 MPa

@Strain 300 %
585 psi

@Strain 300 %
510 mm/min; ASTM D412A
Tensile Strength, Yield 4.24 MPa
615 psi
510 mm/min; ASTM D412A
Elongation at Break 460 %
460 %
510 mm/min; ASTM D412A
Tear Strength 35.0 kN/m
200 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Features General Purpose
Good Melt Strength
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Processing Method Blow Molding
Extrusion
Foam Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: