Polimeri Europa Dutral® TER 4049 Ethylene - Propylene - Diene Terpolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Dutral®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Dutral® TER 4049 Ethylene - Propylene - Diene Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dutral® TER 4049 is an Ethylene - Propylene - Diene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® TER 4049 is a general purpose, high molecular weight amorphous terpolymer of medium diene content. It is characterized by high loading capacity, good mechanical properties, and good collapse resistance. Dutral® TER 4049 based compounds exhibit fast extrusion speed, fast curing, high cure state and excellent low temperature behavior.Main Applications: Automotive, cables, mechanical goods, buildings, appliances.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Mooney Viscosity 76

@Temperature 125 °C
76

@Temperature 257 °F
Ash <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
ENB Content 4.5% wt
Propylene Content 40% wt