Plansee WRe5 Tungsten-Rhenium Alloy

Category Metal , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Plansee SE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee WRe5 Tungsten-Rhenium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics, as compared to pure tungsten:Greater ductilityLower brittle-to-ductile transition temperatureHigher recrystallization temperatureGreater creep resistanceApplications:Thermoelements operating over 2000°CAviation and Aerospace industriesInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 19.4 g/cc
19.4 g/cc
Calculated
Component Elements Properties Metric English Comments
Rhenium, Re 5.0 %
5.0 %
Processing Properties Metric English Comments
Recrystallization Temperature 1700 °C
3090 °F
Deformation level - 90%
Descriptive Properties Value Comments
Creep Resistance greater than pure W
Ductility much greater than pure W
Fineness of Grain comparable to pure W
Machinability/Workability greater than pure W
Stability at High Temperature greater than pure W
Thermal Conductivity less than pure W (164 W/m-K)