Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Piezo Kinetics 502 Lead Zirconate Titanate Piezoelectric

Category Ceramic , Oxide , Titanium Oxide , Zirconium Oxide , Piezoelectric
Manufacturer Piezo Kinetics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Piezo Kinetics 502 Lead Zirconate Titanate Piezoelectric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Denoted as Navy Type II, it is designed for applications that require high electromechanical activity and high dielectric constant. These are used primarily as receivers e.g. hydrophones, phono pickups, sound detectors, accelerometers, delay lines, flow detectors and flow meters.Elastic Compliance s11E (x 10-12 m²/n): 15.4.Elastic Compliance s33E (x 10-12 m²/n): 18.4.Property data at 25°C. Information supplied by Piezo Kinetics, Inc.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 71.0 GPa
10300 ksi
Poissons Ratio 0.31
0.31
Shear Modulus 27.0 GPa
3920 ksi
calculated
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Maximum Operating Temperature
Electrical Properties Metric English Comments
Curie Temperature 350 °C
662 °F
Dielectric Constant 1800

@Frequency 1000 Hz
1800

@Frequency 1000 Hz
Dissipation Factor 0.015

@Frequency 1000 Hz
0.015

@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.69
0.69
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -175
-175
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 580
580
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 25.1
25.1
Piezoelectric Planar Coupling Factor, kp 0.60
0.60
Piezoelectric Mechanical Q 80
80
Piezoelectric Shear Coupling Factor, k15 0.69
0.69
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 400
400
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -11.0
-11.0
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 36.4
36.4
Piezoelectric Transverse Coupling Factor, k31 0.34
0.34
Users viewing this material also viewed the following: