Material Notes:
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance s11E (x 10-12 m²/n): 11.5.Elastic Compliance s33E (x 10-12 m²/n): 15.Property data at 25°C. Information supplied by Piezo Kinetics, Inc.
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 76.0 GPa
11000 ksi
Poissons Ratio 0.31
0.31
Shear Modulus 29.0 GPa
4210 ksi
calculated
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Maximum Operating Temperature
Electrical Properties Metric English Comments
Curie Temperature 350 °C
662 °F
Dielectric Constant 1250

@Frequency 1000 Hz
1250

@Frequency 1000 Hz
Dissipation Factor 0.0050

@Frequency 1000 Hz
0.0050

@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.67
0.67
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -120
-120
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 480
480
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 24.9
24.9
Piezoelectric Planar Coupling Factor, kp 0.52
0.52
Piezoelectric Mechanical Q 500
500
Piezoelectric Shear Coupling Factor, k15 0.68
0.68
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 275
275
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -10.8
-10.8
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 43.4
43.4
Piezoelectric Transverse Coupling Factor, k31 0.33
0.33