Material Notes:
Phenolic - Monsanto "SC 1008". Carbon fabric - "CCA-1"
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 114 MPa
16500 psi
Flexural Yield Strength 183 MPa
26500 psi
Flexural Modulus 15.7 GPa
2280 ksi
Compressive Yield Strength 277 MPa
40200 psi
Compressive Modulus 17.0 GPa
2470 ksi
Users viewing this material also viewed the following: