Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics ParPHorm® L1938-45 Non-Conductive Form-in-Place Gasket

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Parker Chomerics
Trade Name ParPHorm®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics ParPHorm® L1938-45 Non-Conductive Form-in-Place Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material cost versus performance and can provide low cost alternatives for less demanding applications. Chomerics corrosion resistant materials inherently provide protection against galvanic activity. They may eliminate the need for nickel or tin plating and or secondary environmental gaskets. Chomerics general purpose materials exhibit excellent electrical and mechanical properties on metallic and shield plastic housing. Chomerics silver filled materials provide high shielding and conductivity critical for inter-compartmental shields.Features: Lower deflection forces and a broad deflection range, Corrosion resistant materials can eliminate plating or secondary environmental gasket, Good adhesion to many substrates, Supply chain management providing ongoing logistics, and Low cost and rapid prototyping.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
ASTM D2240
Tensile Strength >= 4.25 MPa
>= 616 psi
ASTM D412
Elongation at Break 271 %
271 %
ASTM D412
Compression Set 14 %

@Temperature 70.0 °C,
Time 252000 sec
14 %

@Temperature 158 °F,
Time 70.0 hour
ASTM D395
29 %

@Temperature 100 °C,
Time 252000 sec
29 %

@Temperature 212 °F,
Time 70.0 hour
25% deflection; ASTM D395
29 %

@Temperature 25.0 °C,
Time 7.20e+6 sec
29 %

@Temperature 77.0 °F,
Time 2000 hour
ASTM D395
Processing Properties Metric English Comments
Cure Time 1800 min

@Temperature 140 °C
30.0 hour

@Temperature 284 °F
Tack Free Time
1800 min

@Temperature 140 °C
30.0 hour

@Temperature 284 °F
Handling Time
1800 min

@Temperature 140 °C
30.0 hour

@Temperature 284 °F
Full Cure
Descriptive Properties Value Comments
Color Rust
Resin System Fluorosilicone