Parker Chomerics CHO-BOND 1076, Part A Silicone

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1076, Part A Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 0.800 g/cc
0.800 g/cc
Density 0.00134 g/cc
0.0000484 lb/in³
Vapor Density
Volatiles >= 95 %
>= 95 %
Vapor Pressure 0.125 bar
93.8 torr
Thermal Properties Metric English Comments
Boiling Point 63.9 °C
147 °F
Flash Point >= 93.3 °C
>= 200 °F
Descriptive Properties Value Comments
Physical Form Red Liquid
Silicone Resin % 100
Solubility in Water Soluble