Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pacific Sintered Materials FN-262-T(HT) High Strength Nickel Steel Powdered Metal

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials FN-262-T(HT) High Strength Nickel Steel Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0408-155HTAll information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 37
37
Tensile Strength, Ultimate 1100 MPa
160000 psi
Tensile Strength, Yield 1100 MPa
160000 psi
Elongation at Break <= 0.50 %
<= 0.50 %
Modulus of Elasticity 159 GPa
23000 ksi
Flexural Strength 1690 MPa
245000 psi
Transverse Rupture
Charpy Impact, Unnotched 13.6 J
10.0 ft-lb