Omya OMYACARB® 15 - LU Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name OMYACARB®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYACARB® 15 - LU Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An intermediate, dry ground calcium carbonate with a closely controlled particle size distribution.Applications: Recommended for use in paints, rubber, caulks and sealants, polyester, and plastisol compounds.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
Brightness 91 %
91 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.030 %
0.030 %
Moisture Loss at 110°C % (dry)
Particle Size 15 µm
15 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 1
Retained in 325 mesh (dry), % 9