Northstar Polymers MGA-048 Polyether Prepolymer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers MGA-048 Polyether Prepolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.068 g/cc
1.068 g/cc
Viscosity 900 cP

@Temperature 82.2 °C
900 cP

@Temperature 180 °F
Descriptive Properties Value Comments
Amine Equivalents 480
Appearance at 25°C Pale yellow, waxy solid
NCO (%) 8.75