Nitriflex SB-1009 Styrene Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Nitriflex
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex SB-1009 Styrene Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Used to promote better dimensional stability in articles like profiles, hoses, shoe sole and also recommended to PSA adhesives and adhesives for vertical applications. Available in bale and granules (G). Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 1.0 %
0.00 - 1.0 %
Method B-003; ASTM D5668
Mooney Viscosity 55 - 70

@Temperature 100 °C
55 - 70

@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Linear Mold Shrinkage 0.00 - 0.035 cm/cm
0.00 - 0.035 in/in
ASTM 1917
Ash 0.00 - 1.5 %
0.00 - 1.5 %
ASTM D5667
Chemical Properties Metric English Comments
Styrene Content 21 - 24 %
21 - 24 %
ASTM D5775
Descriptive Properties Value Comments
Appearance Light beige to yellowish