Nitriflex NitriClean 2858 NBR - Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name NitriClean
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex NitriClean 2858 NBR - Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent abrasion resistance, hardness, optimal tensile strength, flexibility at low temperatures and moderate resistance to oils and solvents. Applications: Textile cots, spinning coat, roll covering, safe footwear. Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668
Mooney Viscosity 52 - 64

@Temperature 100 °C
52 - 64

@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Ash 0.00 - 1.0 %
0.00 - 1.0 %
ASTM D5667
Descriptive Properties Value Comments
Appearance White to yellowish
Bound Acrylonitrile Content (%) 27 - 29
ASTM D3533
Mh (lbf.in) 30.0-45.0
ASTM D2084
ML (lbf.in) 9.0-16.0
ASTM D2084
Polymerization Cold
Tsl (min) 1.0-4.0
ASTM D2084