Nihon Superior 95A Sn-Sb Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Nihon Superior
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nihon Superior 95A Sn-Sb Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Properties Metric English Comments
Melting Point 236 - 243 °C
457 - 469 °F
Solidus 236 °C
457 °F
Liquidus 243 °C
469 °F
Component Elements Properties Metric English Comments
Antimony, Sb 5.0 %
5.0 %
Tin, Sn 95 %
95 %
As Remainder