Material Notes:
The addition of lead to this grade permits the production of some 25% more parts with excellent finish and good tool life. Machinability is raised to 145 sfm. Like 4140 annealed, it responds well to heat treatment with good strength and wear resistance, excellent toughness, good ductility in the quenched and tempered condition.Information provided by Niagra LaSalle Corporation
Component Elements Properties Metric English Comments
Carbon, C 0.38 - 0.43 %
0.38 - 0.43 %
Chromium, Cr 0.80 - 1.1 %
0.80 - 1.1 %
Iron, Fe 96.445 - 97.62 %
96.445 - 97.62 %
as balance
Lead, Pb 0.15 - 0.35 %
0.15 - 0.35 %
Manganese, Mn 0.75 - 1.0 %
0.75 - 1.0 %
Molybdenum, Mo 0.15 - 0.25 %
0.15 - 0.25 %
Phosphorous, P <= 0.035 %
<= 0.035 %
Silicon, Si 0.15 - 0.35 %
0.15 - 0.35 %
Sulfur, S <= 0.040 %
<= 0.040 %
Users viewing this material also viewed the following: