Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyolefin
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.932 g/cc
0.932 g/cc
ASTM 792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 6.83 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.83 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
10 seconds; ASTM D2240
Tensile Strength at Break 18.8 MPa
2720 psi
Elastic; ASTM D412
Elongation at Break 720 %
720 %
Elastic; ASTM D412
Flexural Modulus 0.569 GPa
82.5 ksi
Method I (3 point load), Procedure B); ASTM D790
Tear Strength 112 kN/m
640 pli
ASTM D624
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C

@Temperature 20.0 °C
55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696