Mikro-Technik 8036 R/U Carboxymethylcellulose (CMC)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic
Manufacturer Mikro-Technik
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mikro-Technik 8036 R/U Carboxymethylcellulose (CMC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Purified GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special concentrations on request. Most of the grades are available as powder or granules. Special granulometry on request. The viscosity ranges listed above are typical. Narrower ranges and special viscosities are available on request.Information provided by Mikro-Technik GmbH
Physical Properties Metric English Comments
Viscosity 5.0 - 300 cP

@Temperature 20.0 °C
5.0 - 300 cP

@Temperature 68.0 °F
2%, Hoppler
Descriptive Properties Value Comments
Degree of Substitution 0.65
Max. Active Content %, on dry basis 87