Description: One component, water based release coatingUsage: Release Coat® 40 is an easy-to-use one component silicone emulsion coating that provides superior release for a variety of "sticky" products such as hot asphalt. Because it s a one component release system, it eliminates mixing and leftover material disposal. This product is neither hot melt nor cold set gluable.Application Data: Release Coat® 40 may be blade or rod applied at the wet or dry end of the corrugator.Food Contact Information when manufactured in the USA: FDA: 175.105: Components of adhesives. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.02 g/cc
1.00 - 1.02 g/cc
pH 10.4 - 11.4
10.4 - 11.4
Brookfield Viscosity 200 - 625 cP
200 - 625 cP
Spindle # 3, rpm 60
Viscosity Measurement 23 - 33
23 - 33
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance White, opaque liquid
Solids Type Silicone