Mi-Tech Metals Thermitechâ„¢ CW85 85 Tungsten/15 Copper PM Metal Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Mi-Tech Metals
Trade Name Thermitech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mi-Tech Metals Thermitechâ„¢ CW85 85 Tungsten/15 Copper PM Metal Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fully heat treated.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Data provided by Mi-Tech Metals.
Physical Properties Metric English Comments
Density >= 15.9 g/cc
>= 0.574 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 97
97
Component Elements Properties Metric English Comments
Copper, Cu 15 %
15 %
Tungsten, W 85 %
85 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000800 ohm-cm
0.00000800 ohm-cm