Mateck GaAs

Category Other Engineering Material , Semiconductor
Manufacturer Mateck GmbH
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck GaAs.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semiconductor single crystals
Descriptive Properties Value Comments
Carrier Concentration (cm^-3) 1E17-1E19
Doping: None, Type: SI
1E17-1E19
Doping: Si, Type: N
1E17-1E19
Doping: Cr, Type: SI
1E17-1E19
Doping: Te, Type: N
1E17-1E19
Doping: Zn, Type: P
EPD (cm^-2), MAX 100000
Growth Techniques Czochralski. LEC & HB