Material Notes:
Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 12.0 MPa
1740 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 500 %
500 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection