MarkeTech Repton 838 Zirconia + 3 mol% Yttria (YSZ)

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Repton 838 Zirconia + 3 mol% Yttria (YSZ).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Brand 838 features: Co-precipitation; high strength.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Density 6.10 g/cc
0.220 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength >= 1050 MPa
>= 152000 psi
Thermal Properties Metric English Comments
CTE, linear 9.70 µm/m-°C

@Temperature 300 °C
5.39 µin/in-°F

@Temperature 572 °F
10.3 µm/m-°C

@Temperature 900 °C
5.72 µin/in-°F

@Temperature 1650 °F
Component Elements Properties Metric English Comments
Y2O3 3.0 %
3.0 %
ZrO2 97 %
97 %