Material Notes:
Calcium fluoride activated by Europium is light scintillators are used for detection of charged particles and soft gamma ray up to several hundreds keV. CaF:Eu is typically used for detection of beta rays due to its relatively small back scattering. It is not suitable for detection of high-energy gamma ray because has a small photo fraction. It is non hygroscopic and is relatively chemically inert.Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 3.18 g/cc
0.115 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 4.0
4.0
Thermal Properties Metric English Comments
CTE, linear 19.5 µm/m-°C
10.8 µin/in-°F
Melting Point 1360 °C
2480 °F
Descriptive Properties Value Comments
Crystal Structure Cubic
Hydroscopic? No
Luminescence: Afterglow <0.3%
at 6 ms
Luminescence: Decay Constant 940 n/s
Luminescence: Integrated Light Output 50
NaI:Tl = 100
Luminescence: Photon Yield 23
300K; 10<sup>3</sup> pH/MeV
Luminescence: Radiation Length 3.05 cm
Luminescence: Wavelength of max emissions 435 nm