MarkeTech Barium Fluoride, BaF2 Scintillator Crystal

Category Ceramic , Halide
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Barium Fluoride, BaF2 Scintillator Crystal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 4.89 g/cc
0.177 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 3.0
3.0
Thermal Properties Metric English Comments
CTE, linear 18.4 µm/m-°C
10.2 µin/in-°F
Melting Point 1280 °C
2340 °F
Descriptive Properties Value Comments
Crystal Structure Cubic
Hydroscopic? No
Luminescence: Decay Constant 630/0.6 n/s
Luminescence: Integrated Light Output 20/2
NaI:Tl = 100
Luminescence: Photon Yield 10
300K; 10<sup>3</sup> pH/MeV
Luminescence: Radiation Length 2.03 cm
Luminescence: Wavelength of max emissions 325/220 nm