Physical Properties Metric English Comments
Molecular Weight 319.18 g/mol
319.18 g/mol
Descriptive Properties Value Comments
Assay 20% Zn
CAS Number 10139-47-6
Form Off-white crystals
Purity 99.99+%
Typical Impurities Check with Manufacturer