MV Labs SC700 Sc(NO3)3·5H2O Scandium nitrate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SC700 Sc(NO3)3·5H2O Scandium nitrate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 230.97 g/mol
230.97 g/mol
Descriptive Properties Value Comments
Assay 15% Sc
CAS Number 13465-60-6
Form White crystals
Purity 99.999%
Typical Impurities Ca, Zr < 2; Al, Na, Si < 1; Rare Earths < 10 ND