MV Labs SC200 ScBr3·xH2O Scandium bromide hydrate

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SC200 ScBr3·xH2O Scandium bromide hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 284.68 g/mol
284.68 g/mol
Descriptive Properties Value Comments
CAS Number 307496-19-9
Form White crystals
Purity 99.99+%
Typical Impurities Ca, Zr < 2; Al, Na, Si < 1; Rare Earths < 10 ND