MV Labs RH470 [(C6H5)3P]2Rh(CO)Cl Carbonylchlorobis(triphenylphosphine) rhodium(I)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RH470 [(C6H5)3P]2Rh(CO)Cl Carbonylchlorobis(triphenylphosphine) rhodium(I).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 690.96 g/mol
690.96 g/mol
Descriptive Properties Value Comments
Assay 15% Rh
CAS Number 13938-94-8
Form Yellow powder
Purity 99.99+%
Typical Impurities Si < 8; Ir, Pt < 4 ppm