MV Labs PT475 Pt(NH3)2Cl2 trans-Dichlorodiamineplatinum(II)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PT475 Pt(NH3)2Cl2 trans-Dichlorodiamineplatinum(II).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 300.06 g/mol
300.06 g/mol
Descriptive Properties Value Comments
Assay 65% Pt
CAS Number 14913-33-8
Form Pale yellow powder
Purity 99.99+%
Typical Impurities Ca, Cu, Zn = 2; Ag, Fe, Mg, Na, Pt < 1 ppm