MV Labs PT450 (NH4)2PtCl4 Ammonium tetrachloroplatinate(II)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PT450 (NH4)2PtCl4 Ammonium tetrachloroplatinate(II).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 372.98 g/mol
372.98 g/mol
Descriptive Properties Value Comments
Assay 52% Pt
CAS Number 13820-41-2
Form Rose crystals
Purity 99.99+%
Typical Impurities Na = 2; Ag, Al, Ca, Cr, Fe, Si < 1 ppm