MV Labs PR200 PrBr3 Praseodymium bromide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PR200 PrBr3 Praseodymium bromide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 380.63 g/mol
380.63 g/mol
Descriptive Properties Value Comments
Assay 37% Pr
CAS Number 13536-53-3
Form Green crystals
Purity 99.999%
Typical Impurities Ca < 8; Si < 3 ppm; Rare Earths < 10 ND