MV Labs NI410 NiCl2·6H2O Nickel chloride hexahydrate

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NI410 NiCl2·6H2O Nickel chloride hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 237.71 g/mol
237.71 g/mol
Descriptive Properties Value Comments
Assay 25% Ni
CAS Number 7791-20-0
Form Green crystals
Purity 99.9999%
Typical Impurities Cu, Fe, Mg < 1 ppm