MV Labs MN200 MnBr2·4H2O Manganese(II) bromide tetrahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs MN200 MnBr2·4H2O Manganese(II) bromide tetrahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 286.81 g/mol
286.81 g/mol
Descriptive Properties Value Comments
Assay 19% Mn
CAS Number 10031-20-6
Form Pink crystals
Purity 99.999%
Typical Impurities Mg = 3; Fe, Cr = 2; Ca, Ni, Zn < 1 ppm