MV Labs LU500 LuF3 Lutetium fluoride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs LU500 LuF3 Lutetium fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 231.97 g/mol
231.97 g/mol
Descriptive Properties Value Comments
Assay 75% Lu
CAS Number 13760-81-1
Form White powder
Purity 99.99%
Typical Impurities Check with Manufacturer