MV Labs IN700 In(NO3)3·5H2O Indium(III) nitrate pentahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs IN700 In(NO3)3·5H2O Indium(III) nitrate pentahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 390.91 g/mol
390.91 g/mol
Descriptive Properties Value Comments
Assay 31% In
CAS Number 13465-14-0
Form White crystals
Purity 99.999%
Typical Impurities Pb, Bi, Cu, Fe, Mg, Sn < 1 ppm