MV Labs GA800 Ga2O3 Gallium oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs GA800 Ga2O3 Gallium oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 187.44 g/mol
187.44 g/mol
Descriptive Properties Value Comments
Assay 37% Ga
CAS Number 12024-21-4
Form White powder
Purity 99.999+%
Typical Impurities In = 2; Cd, Cr, Cu, Si, Zn < 1 ppm