MV Labs FE400 FeCl2·4H2O Iron(II) chloride tetrahydrate

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs FE400 FeCl2·4H2O Iron(II) chloride tetrahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 198.91 g/mol
198.91 g/mol
Descriptive Properties Value Comments
Assay 28% Fe
CAS Number 13478-10-9
Form Green crystals
Purity 99.999%
Typical Impurities Mn = 5; Co, Cu, Ca = 4; Mg, Ni, Zn < 2 ppm