MV Labs DY1000 Dy2(SO4)3·8H2O Dysprosium sulfate octahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs DY1000 Dy2(SO4)3·8H2O Dysprosium sulfate octahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 757.31 g/mol
757.31 g/mol
Descriptive Properties Value Comments
Assay 42% Dy
CAS Number 10031-50-2
Form Pale yellow powder
Purity 99.999%
Typical Impurities Rare Earths < 10 ND; Ca, Si < 2 ppm