Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs CU200 Cu2Br2 Copper(I) bromide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CU200 Cu2Br2 Copper(I) bromide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 286.9 g/mol
286.9 g/mol
Descriptive Properties Value Comments
Assay 44% Cu
CAS Number 7787-70-4
Form Pale yellow powder
Purity 99.999%
Typical Impurities Ag, Fe, Mg, Pb, Si = 1 ppm
Users viewing this material also viewed the following: