MV Labs CU110 Cu(C2H3O2)2 Copper(II) acetate, anhydrous

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CU110 Cu(C2H3O2)2 Copper(II) acetate, anhydrous.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 181.63 g/mol
181.63 g/mol
Descriptive Properties Value Comments
Assay 35% Cu
CAS Number 142-71-2
Form Blue crystals
Purity 99.999%
Typical Impurities Mg, Pb, Si = 1 ppm