MV Labs CA870 CaC2O4 Calcium oxalate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CA870 CaC2O4 Calcium oxalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 128.1 g/mol
128.1 g/mol
Descriptive Properties Value Comments
Assay 31% Ca
CAS Number 563-72-4
Form White powder
Purity 99.999%
Typical Impurities Sr = 5; Na = 2; Cu, Fe, Mg, Mn, Si < 1 ppm