MV Labs AL850 ((CH3)2CHO)3Al Aluminum isopropoxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AL850 ((CH3)2CHO)3Al Aluminum isopropoxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 204.25 g/mol
204.25 g/mol
Descriptive Properties Value Comments
Assay 13% Al
CAS Number 555-31-7
Form white powder
Purity 99.99+%
Typical Impurities Fe, K = 30; Si, Na, Mn = 15; Zn, Ca, Mg = 5; Cd, Ba, Cr, Co, Cu, Ni < 1 ppm